Pono
- Pololei loa
- Ke kino ʻili maikaʻi
- Maʻemaʻe nā kihi a me nā kihi
- Kūleʻa maikaʻi i ka wai
Nā noi kūpono
- Nā hiʻohiʻona kāmaʻa
- niho
- Art a me ka hoʻolālā
- Kii
- Kiʻi ʻoniʻoni
Pepa ʻikepili ʻenehana
Waiwai Waiwai | ʻAno Optical | ||
Ka nana aku | Palaunu | ʻO Dp | 0.135-0.155 mm |
ʻO ka viscosity | 405-505 cps @ 28 ℃ | Ec | 9-12 mJ/cm2 |
ʻO ka mānoanoa | 1.11-1.14g/cm3 @ 25 ℃ | Mānoanoa papa hale | 0.1-0.15mm |
Na Waiwai Mechanical | UV Postcure | |
ANA | ANOAI HOAO | WAIWAI |
Paʻakiki , Kahakai D | ASTM D 2240 | 74-80 |
Pākuʻi hoʻololi , Mpa | ASTM D 790 | 2,650-2,750 |
Ka ikaika wiliwili , Mpa | ASTM D 790 | 60- 75 |
ʻO ka modulus tensile , MPa | ASTM D 638 | 2,150-2,370 |
Ka ikaika tensile , MPa | ASTM D 638 | 25-30 |
Elongation i ka wā hoʻomaha | ASTM D 638 | 12 -20% |
Ka ikaika o ka hopena, ka lzod notched, J/m | ASTM D 256 | 58 - 70 |
ʻO ka wela wela, ℃ | ASTM D 648 @66PSI | 58-68 |
Hoʻololi aniani, Tg | DMA,E” peak | 55-70 |
ʻO ka mānoanoa , g/cm3 | 1.14-1.16 |
ʻO ka mahana i manaʻo ʻia no ka hana ʻana a me ka mālama ʻana i ka resin ma luna nei he 18 ℃-25 ℃.