I-PX 223/HT

Incazelo emfushane:

I-Vacuum Casting Polyurethane Resin Yezingxenye Zobuchwepheshe kanye Nezibonelo I-Flexural Modulus 2,300 Mpa – Tg 120°c


Imininingwane Yomkhiqizo

Omaka bomkhiqizo

IZICELO

Isetshenziswa ngokufaka isikhunta se-silicone ukuze kufezeke izingxenye ze-prototype kanye nama-mock-ups anomshini

izakhiwo ziseduze nalezo ze-thermoplastics.

 

IZIMPAHLA

Phansi i-viscosity okwe kulula ukuphonsa

Kuhle umthelela futhi eguquguqukayo ukumelana

Izinga lokushisa ukumelana ngenhla 120°C

EMZIMBENI IZIMPAHLA
    INGXENYE A INGXENYE B I-MIXING
Ukwakheka   ISOCYANATE PI-OLYOL  
Ukuhlanganisa isilinganiso ngesisindo ku-25°C   100 80  
Isici   uketshezi Uketshezi uketshezi
Umbala   engenambala mnyama mnyama
I-Viscosity ku-25°C (mPa.s) Izindleko zamasheya BROOKFIELD LVT 1.100 300 850
Ukuminyana kwezingxenye ngaphambi kokuxuba ku-25°C Ukuminyana kokuxuba okuphulukisiwe ku-23°C ISO 1675 :1975 ISO 2781 :1988 1.17

-

1.12

-

-

1.14

Impilo yebhodwe ku-25°C ku-90g (amaminithi.) -     6-7

UKUQHUBEKA (Umshini wokukhipha ivacuum)

Vacuum ukuphonsa phakathi i-silicone isikhunta.

Kokubili izingxenye babe to be kusetshenziwe at a izinga lokushisa ngenhla +18°C.

   Okubalulekile : Rehomogenize ingxenye B ngaphambili ngamunye ukukala.

I-Degas ngamunye ingxenye ngaphambili sebenzisa.

Hlanganisa okwe 45 imizuzwana cishe.

Abalingisi in a isikhunta ngaphambili-eshisiwe at 40°C ubuncane.

Vumela to ukwelapha 45 to 75 imizuzu at 70°C ngaphambili ukudiliza

Thwala ngaphandle i kulandela ezishisayo ukwelashwa : 1 hr at 100°C + 2 hr at 110°C or Okuningi if kungenzeka.

QAPHELA :  Ngemva ukudiliza it is hhayi okudingekayo to sebenzisa a umfanisi to gcina i ingxenye in i ihhavini ngesikhathi i okuthunyelwe

UKUPHATHA IZIQINISEKISO

Okuvamile impilo futhi ukuphepha izinyathelo zokuzivikela kufanele be kubhekwe nini ukuphatha lezi imikhiqizo :

qinisekisa kuhle ukungena komoya

gqoka amagilavu futhi ukuphepha izibuko

Ngoba ngokuqhubekayo ulwazi, Ngiyacela bonisana i umkhiqizo ukuphepha idatha ishidi.

Ikhasi 1/ 2- 21 Mar. 2007

I-AXSON France AXSON GmbH AXINDODANA IBERICA I-AXSON AI-SIA I-AXSON JI-PAN I-AXSON SI-HANHAI
Idatha ye-BP40444 I-Dietzenbach Barcelona I-Seoul OKAZAKI CITY

Inombolo yepholisi: 200131

95005 Cergy Cedex Ucingo.(49) 6074407110 Ucingo.(34) 932251620 Ucingo.(82) 25994785 Ucingo.(81)564262591

Shanghai

I-FRANCE Ucingo.(86) 58683037
Ucingo .(33) 134403460 I-AXSON IsiNtaliyane I-AXSON UK AXINDODANA EMEXICO AXINDODANA NA USA Ifeksi.(86) 58682601
Ifeksi (33) 134219787 Saronno Newmarket I-Mexico DF I-Eaton Rapids E-mail: shanghai@axson.cn
I-imeyili :axson@axson.fr Ucingo.(39) 0296702336 Ucingo.(44)1638660062 Ucingo.(52) 5552644922 Ucingo.(1) 5176638191 Iwebhu:http://www.axson.com.cn

I-Vacuum Casting Polyurethane Resin Yezingxenye Zobuchwepheshe kanye Nezibonelo I-Flexural Modulus 2,300 Mpa - Tg 120°c

MI-ECHANICAL IZIMPAHLA AT 23°C(1)
I-Flexural modulus ye-elasticity ISO 178 :2001 I-MPa 2.300
Amandla e-Flexural ISO 178 :2001 I-MPa 80
Amandla aqinile ISO 527 :1993 I-MPa 60
Ukwelula ngesikhathi sekhefu ISO 527 :1993 % 11
Ukumelana nomthelela we-Charpy ISO 179/2D :1994 kJ/m2 > 60
Ukuqina - ku-23°C- ku-120°C ISO 868:1985 Ugu D1 80> 65

 

OKUSHISAYO KANYE OKUQONDILE IZIMPAHLA(1)
Izinga lokushisa lokushintsha kwengilazi I-TMA-Mettler °C > 120
I-coefficient ye-linear thermal expansion (CLTE) [+15, +120]°C I-TMA-Mettler ppm/K 115
Ukuncipha komugqa - mm/m 4
Ubukhulu bokulingisa obukhulu - mm 5-10

(1) : Amanani amaphakathi atholwe kuma-specimens ajwayelekile / Ukuqina ihora elingu-1 ngo-70°C + 1 ihora ku-100°C + 12 hr ku-110°C

ISITOREJI CONDITIONS

Isikhathi seshelufu sazo zombili izingxenye siyizinyanga eziyi-12 endaweni eyomile futhi ezitsheni zazo zasekuqaleni ezingavuliwe ezingeni lokushisa eliphakathi kuka-15 no-25°C.Noma yiliphi ithini elivuliwe kufanele livalwe ngokuqinile ngaphansi kwengubo eyomile ye-nitrogen.

UKUPAKASHA

ISOCYANATE (Ingxenye A)
1 × 1.0 kg
1 × 5.0 kg

POI-LYOL (Ingxenye B)
1 × 0.8 kg
1 × 4.0 kg 

A + B
5 × (1+0.8) kg
6 × (1+0.8) kg

I-GUARAI-NTEE

Ulwazi oluqukethwe kuleli phepha ledatha yobuchwepheshe luvela ocwaningweni nasezivivinyweni ezenziwa eLabhorethri yethu ngaphansi kwezimo eziqondile.Kuyisibopho somsebenzisi ukunquma ukufaneleka kwemikhiqizo ye-AXSON, ngaphansi kwemibandela yakhe ngaphambi kokuqala ngohlelo lokusebenza oluhlongozwayo.I-AXSON iqinisekisa ukuhambisana kwemikhiqizo yabo nezicaciso zayo kodwa ayikwazi ukuqinisekisa ukuhambisana komkhiqizo nanoma yiluphi uhlelo lokusebenza.I-AXSON iyakulahla konke ukubophezeleka komonakalo kunoma yisiphi isigameko esiwumphumela wokusetshenziswa kwale mikhiqizo.Isibopho se-AXSON sikhawulelwe ngokuphelele ekubuyiseleni noma ukushintshwa kwemikhiqizo engahambisani nezicaciso ezishicilelwe.

(1) Amanani amaphakathi atholwe kuma-specimens ajwayelekile/Ukuqina amahora ayi-12 ku-70°C

ISITOREJI

Isikhathi seshelufu yizinyanga eziyisi-6 INGXENYE A (Isocyanate) kanye nezinyanga eziyi-12 INGXENYE B (Polyol) endaweni eyomile nasezitsheni zasekuqaleni ezingavuliwe ezingeni lokushisa eliphakathi kuka-15 no-25° C. Noma iyiphi ithini evuliwe kufanele ivalwe ngokuqinile ngaphansi kwengubo eyomile ye-nitrogen. .

QINISEKISA

Ulwazi lweshidi lethu ledatha yobuchwepheshe lusekelwe olwazini lwethu lwamanje kanye nomphumela wokuhlolwa okwenziwa ngaphansi kwezimo eziqondile.Kuyisibopho somsebenzisi ukunquma ukufaneleka kwemikhiqizo ye-AXSON, ngaphansi kwemibandela yakhe ngaphambi kokuqala ngohlelo lokusebenza oluhlongozwayo.I-AXSON yenqaba noma isiphi isiqinisekiso mayelana nokuhambisana komkhiqizo nanoma yiluphi uhlelo lokusebenza oluthile.I-AXSON iyakulahla konke ukubophezeleka komonakalo kunoma yisiphi isigameko esiwumphumela wokusetshenziswa kwale mikhiqizo.Izimo zesiqinisekiso zilawulwa yimibandela yethu yokuthengisa evamile.