Kaluwihan
Resistance suhu dhuwur
Stabilitas dimensi sing apik banget
Kekuwatan lan akurasi sing dhuwur
Aplikasi Ideal
Prototipe mbutuhake tahan suhu dhuwur
Cetakan cepet
Lembar data teknis
Sifat Cairan | Sifat Optik | |||
Penampilan | Semi-translucent | Dp | 13,5 mJ/cm2 | [ekspos kritis] |
Viskositas | 340 cps@30 ℃ | Ec | 0,115 mm | [slope of cure-depth vs. In (E) curve] |
Kapadhetan | 1,14 g/cm3 | Ketebalan lapisan bangunan | 0,08-0,12 mm |
Sifat mekanik | UV post curing | |||
Item tes | Metode Tes | Nilai angka | Metode Tes | Nilai angka |
Kekuwatan Tensile | ASTMD 638 | 65MPa | GB / T1040.1-2006 | 71MPa |
Elongation ing break | ASTMD 638 | 3-5% | GB / T1040.1-2006 | 3-5% |
Kekuwatan mlengkung | ASTMD 790 | 110MPa | GB / T9341-2008 | 115MPa |
Modulus lentur | ASTMD 790 | 2720MPa | GB / T9341-2008 | 2850MPa |
Izod notched impact kekuatan | ASTMD 256 | 20J/m | GB / T1843-2008 | 25J/m |
Kekerasan pantai | ASTMD 2240 | 87D | GB / T2411-2008 | 87D |
Suhu transisi kaca | DMA, tan θ puncak | 135 ℃ | ||
Koefisien ekspansi termal (25-50 ℃) | ASTME831-05 | 50 µm/m ℃ | GB / T1036-89 | 50 µm/m ℃ |
Koefisien ekspansi termal (50-100 ℃) | ASTME831-05 | 150 µm/m ℃ | GB / T1036-89 | 160 µm/m ℃ |
Rekomendasi suhu kanggo Processing lan panyimpenan saka resin ndhuwur kudu 18 ℃ -25 ℃.